Shift is a casting defect which$?

Question Bank Mechanical Engineering 1 year ago

1.94K 1 0 0 0

Option 1 : Results in a mismatching of the top and bottom parts of a casting

Option 2 : Results in general enlargement of a casting

Option 3 : Occurs near the ingates as rough lumps on the surface of a casting

Option 4 : Occurs as sand patches on the upper surface of a casting


 

Click Here For the Answer

User submissions are the sole responsibility of contributors, with TuteeHUB disclaiming liability for accuracy, copyrights, or consequences of use; content is for informational purposes only and not professional advice.

Answers (1)

Post Answer
profilepic.png
ZakjexZK ZakjexZK Tuteehub forum best answer Best Answer 1 year ago
Results in general enlargement of a casting


Click Here For More

0 views
0 shares

No matter what stage you're at in your education or career, TuteeHUB will help you reach the next level that you're aiming for. Simply,Choose a subject/topic and get started in self-paced practice sessions to improve your knowledge and scores.

Similar Forum


Q

Many a times we read in the newspapers that in India, while rice (non-basmati) exports are banned, b...

Option 1 : Modified Export ProvisionsOption 2 : Maximum Export Permission Option 3 : Minimum Export...
Q

Which among the following duties is applied by a Government to control the exports of a commodity, s...

Option 1 : Custom Duty Option 2 : Excise DutyOption 3 : Anti Dumping Duty Option 4 : Dumping Duty &n...
Q

A person lost his job due to economic recession. He agreed to do some job on a low wage. This is kno...

Option 1 : Seasonal Unemployment Option 2 : Cyclical Unemployment Option 3 : Disguised Unemployment...